Materials
-
High Performance > 300°F
- Polyetheretherketone (PEEK)
- Polyphenylene Sulfide (PPS)
- Polyetherimide (Ultem®)
- Sulfones
-
Engineering 185°F - 300°F
- Acetal
- Nylon
- Polyesters
- Polycarbonate
- Polyphenylene Oxide (PPO)
- Polyvinylidene Fluoride (PVDF)
-
General Industrial < 185°F
- Polypropylene
- Polyethylene
- Acrylonitrile Butadiene Styrene
Certification
TECASON P Polyphenylsulfone
Offering a level of performance above polysulfones, TECASON™P has increased temperature, impact and chemical resistance properties as well as excellent resistance to repeated steam sterilization (autoclave) cycles.
TECASON™ P is a polyphenylsufone that exhibits excellent temperature, impact and chemical resistance properties.
Properties | Condition | Value | Test Method | Comment | ||||
---|---|---|---|---|---|---|---|---|
Mechanical | Modulus of elasticity (tensile test) | @ 73 °F | 340,000 | psi | ASTM D 638 | |||
Tensile strength at yield | @ 73 °F | 10,100 | psi | ASTM D 638 | ||||
Elongation at break | @ 73 °F | 60 | % | ASTM D 638 | ||||
Modulus of elasticity (flexural test) | @ 73 °F | 350,000 | psi | ASTM D 790 | ||||
Compression strength | @ 73 °F | 14,350 | psi | ASTM D 695 | ||||
Impact strength (Izod) | @ 73 °F | 13 | ft-lbs/in | ASTM D 256 | ||||
Rockwell Hardness | @ 73 °F R Scale | 123 | ASTM D 785 | |||||
Thermal | Vicat softening point | 424 | °F | 1) | 1) Injection Molded Sample | |||
Deflection temperature | @ 264 psi | 420 | °F | ASTM D 648 | ||||
Deflection temperature | @ 66 psi | 428 | °F | ASTM D 648 | ||||
Service temperature | Intermittent | 360 | °F | |||||
Thermal expansion (CLTE) | 1.7*10-5 | in/in/°F | ASTM D 696 | |||||
Specific heat | 0.27 | BTU/lb-F° |
||||||
Thermal conductivity | 1.74 | BTU-in/hr-ft2-°F | - | |||||
Electrical | Volume resistivity | 1*1015 | Ω*cm | ASTM D 257 1) | ||||
Dielectric Strength | 360 | V/mil | ASTM D 149 | |||||
Dielectric constant | @ 60Hz, 73 °F, 50% RH | 3.44 | ASTM D 150 | |||||
Other | Moisture absorption | @ 24 hrs, 73 °F | 0.37 | % | ASTM D 570 | |||
Moisture absorption | @ saturation, 73 °F | 1.1 | % | ASTM D 570 | ||||
Flammability (UL94) | V-0 | 2) | 2) Injection molded sample thickness greater than 0.790 mm | |||||
This information is only to assist and advise you on current technical knowledge and is given without obligation or liability. All trade and patent rights should be observed. All rights reserved. Data obtained from extruded shapes material. |